Journal of Dental Rehabilitation and Applied Science:eISSN 2384-4272 pISSN 2384-4353

Fig. 7.

Download original image
Scanning electron microscope (SEM) photographs after shear bond strength test: Mixed failure. (A) Group NT (NextDent + Tokuyama rebase II): Mixed failure (x50), (B) Group NT (NextDent + Tokuyama rebase II): Mixed failure (x1000).
J Dent Rehabil Appl Sci 2021;37:232-43 https://doi.org/10.14368/jdras.2021.37.4.232