Table. 2.

Table. 2.

Kruskal-Wallis test with Zirconia Thickness, zirconia shade and background

Factor X2 Df P-value
Thickness 172.116 3 0.000*
Zirconia shade 256.571 1 0.000*
Background 81.395 4 0.000*

The symbol (*) represents statistical significant difference (P<0.05).

J Dent Rehabil Appl Sci 2021;37:199-208 https://doi.org/10.14368/jdras.2021.37.4.199