Table. 5.

Table. 5.

Results of Tukey HSD test on shear bond strengths

UM UE UC PM PE PC
UM
UE .385
UC < .001 * < .001 *
PM .097 .978 < .001 *
PE .056 .929 < .001 * 1.000
PC .001 .154 .039 * .516 .663

* denotes significant difference between groups (P < 0.05).

J Dent Rehabil Appl Sci 2020;36:1-11 https://doi.org/10.14368/jdras.2020.36.1.1